Researchers at University of Virginia used operando TEM to study pitting corrosion in stainless steel.
Using a Protochips #PoseidonSelect they performed liquid-TEM studies during applied potentiodynamic polarization and observed the dissolution of MnS in inclusions in a lamella of 304L stainless steel.
Read their paper published in Corrosion Science here: https://lnkd.in/g5yUxGwv.